Lime screed in a timber frame house: planning and professional execution on sandy ground
Renovating a timber frame house confronts builders and planners with a fundamental decision: which floor build-up makes sense in terms of building physics and is at the same time compatible with the historic building fabric? Modern concrete slabs and cement screeds seem stable and familiar at first, but in historic buildings they can lead to moisture problems in the long term. A mineral floor build-up with lime screed is the much better solution.
Lime screed for your floor
KHOLAO CHAPE from Saint-Astier, a lime screed without cement for old buildings and timber frame houses. Enter the floor area; the list calculates the quantity.
- Saint-Astier® KHOLAO® Chape lime screed 50 × standard801,50 €
Total for 15 m²801,50 €
incl. VAT, plus shipping
Plus on site, not in the list
- Substrate of lime concrete (Saint-Astier NHL 5 with gravel sand 0/16, from about 15 cm), load-bearing old concrete or hempcrete
- Edge insulation strip all round
Why lime screed instead of cement screed in a timber frame house?
A lime screed combines several decisive properties: it is vapour-permeable, capillary-active, low in stress and compatible with traditional building materials. Especially in timber frame houses with a sandy subsoil, such a build-up can work permanently, provided planning and execution are correct.
Taking regional ground conditions into account is particularly important here. In northern Germany, sandy soils, fluctuating groundwater levels and sometimes pressing groundwater are typical. These conditions require careful planning of the floor build-up. Natural hydraulic limes such as the products from Saint Astier have proven themselves here for decades because they are sufficiently moisture-resistant and at the same time remain vapour-permeable.
Cement, on the other hand, has a very dense structure. It blocks moisture and can therefore cause massive problems in historic buildings: moisture is trapped in the floor, rises capillarily into the timber frame walls and encourages timber rot and mould. A lime screed, by contrast, allows capillary-active and vapour-permeable moisture transport in keeping with historic construction.
Building physics basics: how a lime screed hardens
Lime screeds differ fundamentally from cement screeds. While cement mortar hardens through a hydration reaction and then becomes very dense, a lime screed hardens through two processes.
The first process is the hydraulic reaction: natural hydraulic limes contain natural silicates that react with water and produce initial strength. The second process is carbonation, in which calcium hydroxide from the lime reacts with carbon dioxide from the air and forms calcium carbonate, i.e. limestone. This process strengthens the screed in the long term and can take several months.
This dual hardening produces a stable yet vapour-permeable structure. Typical properties of a lime screed are vapour permeability, capillary activity, low stress and complete repairability. Depending on the mix, the bulk density is usually between about 1.600 and 2.000 kg per cubic metre, somewhat lower than cement screeds, which explains the lower brittleness and better compatibility with the flexible timber structure.
Special requirements in timber frame houses
In terms of building physics, timber frame houses are constructed differently from modern buildings. Historic constructions were built without vapour barriers and without waterproof concrete slabs. Moisture could therefore always diffuse through materials and be carried downwards or sideways.
A functioning floor build-up must therefore meet the following requirements: vapour permeability, capillarity, moisture tolerance and low stress. Rigid and dense materials such as concrete or cement can cause problems in this system. If moisture from the ground cannot escape downwards, it often rises into the timber frame walls, with consequences for the timber structure, the panels and the plaster.
A lime screed, by contrast, fits into the historic building system. It allows moisture to take the route it should take in a historic building: diffusely through the layers and capillarily into and out of the open-pored materials.
Regional differences: northern Germany and sandy soils
Geological conditions in Germany differ greatly and considerably influence the planning of a floor build-up. In northern Germany, sandy soils, glacial sands and glacial deposits dominate. These soils are highly permeable to water, and rainwater seeps away quickly. At the same time, groundwater levels can fluctuate considerably by region. Pressing groundwater can occur particularly in coastal regions, river lowlands and marshes.
In such situations, a mineral floor build-up is only possible if functioning drainage is in place. Without drainage, water can stand permanently under the screed and destabilise the construction. A correctly planned lime screed therefore needs drainage layers, capillary-breaking materials and, if necessary, drainage lines.
In central and southern Germany, loam, clay and loess occur more frequently as soil types. These soils store water more strongly and have much higher capillarity. As a result, moisture can be held in the ground for longer. Here a capillary-breaking layer is particularly important to reduce rising damp. The build-up of a lime screed is similar in both regions, but the dimensioning of the individual layers and the decision on drainage lines depend heavily on local ground conditions.
Layer build-up of a lime screed: from drainage to surface
Preparing the substrate
A functioning lime screed floor consists of several layers, each fulfilling a specific building physics task. The first step is exposing the load-bearing subsoil. The floor is excavated down to firm ground. This must be load-bearing, even and free of organic components. On sandy soils, light compaction with a vibrating plate or hand tamper is often enough. On clayey soils, additional stabilisation may be required.
The drainage layer is built from gravel or crushed stone with a grain size of about 16 to 32 mm, in a layer thickness of about 20 to 30 cm. In regions with a high water table, a drainage line is also recommended: a perforated drainage pipe embedded in a gravel bed and connected to a drain.
Above the drainage layer follows a capillary-breaking layer of foam glass gravel, coarse gravel or expanded clay. These materials have large pore spaces, so water cannot be transported upwards by capillary action. Typical layer thickness: 10 to 15 cm. The grain size should be at least 4 to 8 mm so that capillary effects are reliably interrupted.
A mineral base layer is placed on the capillary-breaking layer. Historically, rammed earth, clay gravel or lime gravel was used for this. Today a lime gravel mix of one part hydraulic lime and four to six parts gravel or sand is used. The leaner the mix, the more capillary-active the layer remains. Suitable binders are natural hydraulic limes such as Saint Astier NHL 3,5 or NHL 5.
Choice of material: which hydraulic lime is suitable for lime screed?
The screed itself is also made of natural hydraulic lime. Saint Astier NHL 3,5 is suitable for normal residential loads. NHL 5 has higher strength and is used for higher moisture loads, more heavily stressed floors and workshop or utility areas. These natural limes have been used in European monument conservation for centuries and were developed specifically for historic constructions exposed to moisture.
A typical mixing ratio for lime screed is 1 part hydraulic lime to 3 parts sand (by volume). With NHL 5, mixes between 1:3 and 1:4 are often used. The sand should be well graded, typical grain size 0 to 8 mm. The sand must be washed and free of clay and organic components. Impurities reduce strength and can impair vapour permeability.
Lime screed is usually laid in a layer of about 6 to 10 cm. For heavier loads, the layer can also be up to 12 cm. The screed is then spread, levelled and lightly compacted. Excessive compaction should be avoided. It reduces porosity and thus the diffusion capacity of the screed.
Drying, carbonation and surface treatment
A lime screed hardens much more slowly than cement screeds. Hydraulic hardening typically takes about 2 to 4 weeks. After that the screed can usually be walked on carefully. Complete carbonation, however, can take several months. The speed depends on temperature, humidity, the CO₂ content of the air and the layer thickness. During this time the screed should be protected from drying out too quickly, for example by covering it with damp cloths.
Lime screeds can be finished in different ways: as a smoothly levelled screed, as lime filler, with a brick covering or a natural stone covering. Oiled lime screeds are also possible and give the floor a protective, water-repellent surface without completely removing vapour permeability. The surface of a lime screed becomes firmer and more resistant over time through use and carbonation.
Combination with clay plaster in a timber frame house
In many timber frame houses, lime screed is combined with clay building products. A typical build-up has clay plaster on the interior walls, lime screed on the floor and lime plaster on the facade. This combination creates a fully mineral and vapour-permeable building envelope that consistently continues the historic building system.
ClayTec products are particularly suitable for clay plasters indoors. The combination of ClayTec clay plaster and Saint Astier lime screed creates a fully mineral and vapour-permeable building envelope. All materials are matched to each other, have comparable elasticity and react compatibly in terms of building physics to changes in temperature and moisture.
At Lehm-Revival you will find exactly these materials in tested quality. Lime products from Saint Astier and the complete ClayTec range of clay plasters and clay paints are available, matched to the requirements of timber frame renovation in northern Germany.
Common mistakes with lime screeds and how to avoid them
In practice, problems with lime screeds are almost always caused by wrong planning or the wrong choice of material. The most common mistake is missing drainage: without a drainage layer, water can stand permanently under the screed. In the long term this leads to moisture damage, detachment and cracking.
Another common mistake is omitting the capillary-breaking layer. Without it, moisture rises capillarily through the floor layers into the screed. Using cement mortar as an admixture or as binder for the base layer is also problematic. Even small amounts of cement can considerably reduce vapour permeability.
Drying too quickly is also a typical mistake. If lime screed dries out too quickly, for example due to direct sunlight or strong heating indoors, shrinkage cracks develop that weaken the screed. Freshly laid lime screed should therefore be kept damp for at least two to three weeks, for example by covering or careful watering.
| Layer | Material | Thickness approx. | Note |
|---|---|---|---|
| Substrate | Load-bearing ground, compacted | depending on the subsoil | Plate compactor or hand rammer |
| Drainage layer | Gravel / crushed stone 16–32 mm | 20–30 cm | If necessary, drainage pipe with a high groundwater level |
| Capillary-breaking layer | Foam glass gravel, expanded clay, coarse gravel ≥ 4 mm | 10–15 cm | The capillary effect must be reliably interrupted |
| Base layer | Saint Astier NHL 3,5 or NHL 5 : gravel (1:4–6) | 10–15 cm | The leaner, the more capillary-active |
| Lime screed | Saint Astier NHL 3,5 or NHL 5 : sand 0–8 mm (1:3) | 6–10 cm | Up to 12 cm under higher loads |
| Surface (optional) | Lime filler, natural stone, brick or oiled lime screed | — | Remaining vapour-permeable |
Regional context and use in practice
In northern Germany, especially in the lowland landscape between Achim, Verden, Rotenburg (Wümme) and the coast, sandy soils and fluctuating groundwater levels are typical. Timber frame houses in this region need a carefully planned mineral floor build-up. Lehm-Revival at Danziger Str. 59, 28832 Achim advises homeowners and craft businesses on planning and material selection for lime screeds and delivers Saint Astier natural limes and ClayTec clay products by parcel or haulier.
Gently exposing timber frame beams: blasting removes old coatings and incrustations without residue, without chemicals, without damaging the wood fibres.
Blast timber framingOpen questions
Which build-up belongs under a lime screed in a timber frame house?
From bottom to top: load-bearing, compacted subsoil, a drainage layer of gravel or crushed stone (grain size 16 to 32 mm) of about 20 to 30 cm, a capillary-breaking layer of foam glass gravel, expanded clay or coarse gravel of 10 to 15 cm and a base layer of hydraulic lime with gravel. On top comes the screed at 6 to 10 cm. With a high water table, a drainage pipe is added. Missing drainage and a missing capillary-breaking layer are the most common causes of damage.
Saint-Astier NHL 3,5 or NHL 5: which lime for the screed?
NHL 3,5 is suitable for normal residential loads. NHL 5 achieves higher strength and is used for higher moisture loads, more heavily stressed floors and workshop and utility areas. Both natural limes remain vapour-permeable and suit historic construction.
How long does it take for a self-mixed NHL lime screed to harden?
Hydraulic hardening typically takes 2 to 4 weeks, after which the screed can be walked on carefully. Carbonation, the second hardening process, can take several months; only then does the screed reach its full strength. Keep fresh lime screed damp for at least two to three weeks, for example by covering it, and protect it from direct sun and strong heating.
Can I make and lay lime screed myself?
Experienced DIYers can lay simple lime screeds in small areas themselves. It is important to keep to the right mixing ratio (1:3 lime to sand) and to let the screed dry sufficiently slowly. For larger areas, more heavily stressed floors or more complicated floor conditions, I recommend working with a specialist company experienced with lime screeds in historic buildings.
Sources and standards
Further links
Products in the shop
Knowledge articles
More items in Timber framing & wood
- Building physics for natural building materials: vapour diffusion, heat storage and dew point
- Timber frame wall build-up: layers, materials and structure fully explained
- Filling a timber frame panel: definition, materials and step-by-step guide
- Timber framing in central Germany: history, construction methods and regional features
- Timber framing in northern Germany: history, construction methods and regional features
- Renovating timber framing with clay: step by step to a healthy timber frame wall
- Timber framing in southern Germany: history, construction methods and regional features
- Historic roof windows in listed buildings: permit, models and installation
- Lime in timber frame construction: using NHL and alpine lime
- Clay in timber framing: infill, plaster and renovation
- Clay vs. brick in timber framing: which material really suits the panels?
- Filling a panel: clay block or hemp block in timber framing
- Clay-wrapped staves in timber framing: historic restoration, reuse and professional new production
- What is timber framing? Structure, function and materials simply explained
- Reusing old bricks in timber framing: cleaning, triangular battens and professional reinstallation
To take away: the free clay building diary with drying log.
Download free of charge