Skip to main content

Reusing old bricks in timber framing: cleaning, triangular battens and professional reinstallation

Kenny Kent BridgewaterFromKenny Kent BridgewaterExpert for resource-efficient and sustainable buildingAs of:

Old bricks from timber frame panels can be reused in many cases, but not automatically. The decision depends on specific test criteria: cracks, frost damage, salt contamination and the sound test provide the relevant clues. This article shows which bricks are really suitable for reinstallation, how the test works, which damage speaks against reuse and when replacement with new bricks is the better decision.

Reuse check matrix: old bricks in timber framing

These 6 check points decide on continued use or replacement before the renovation

CheckpointReuse possible if…Replacement necessary if…
Cracks and breaksNo cracks, intact edgesContinuous cracks, broken halves
Frost damageSurface smooth and hardPeeling, flaking
Salt efflorescenceNo visible efflorescenceWhite crusts, salt crystals visible
Joint adhesionsLime comes off easilyCement joint, brick splinters when cleaning
Compression test (hand)No loss of material under pressureSoft, crumbly, sanding
Original provenanceHistoric fired solid brickModern perforated brick, geometrically unsuitable
Lehm-Revival employee cleaning an old brick with a natural bristle brush over a grating in a timber frame room, preparing historic bricks for reinstallation
Brush off lime mortar residues over the grating: a natural bristle brush protects the open-pored surface and ensures adhesion on reinstallation.
Check matrix: assessing the suitability of bricks before reinstallation
CheckpointFeature / damageRatingRecommendation
Cracks and breaksContinuous cracks, broken halves, heavily broken-out areasNot suitableSort out, no structural integrity
Edge chipping (small)Individual mortar imprints, superficial spalling at edgesSuitableInstall, affects only the surface, not the core structure
Sound testDull, hollow sound when two bricks are knocked togetherNot suitableSort out, indicates internal cracks or frost damage
Sound testBright, clear sound when two bricks are knocked togetherSuitableInstall, block structurally intact
Frost damagePeeling surfaces, bursting layers, crumbly edgesNot suitableSort out, pore structure irreversibly destroyed
Salt contamination (efflorescence)White deposits on the surface, salt efflorescencePartly suitableInstall after complete drying, not in damp areas
Dimensional deviationFormat differs greatly from the remaining stockPartly suitableSet aside for less visible areas or inner layers
Mortar residues after cleaningMortar residues completely removed, clean surfaceSuitableInstall, cleaning completed, adhesion ensured

Building physics basis: why historic bricks are particularly suitable in timber framing

Historic bricks were fired at lower temperatures than modern industrial bricks. The result is an open-pored structure that absorbs, transports and releases moisture: capillary-active and vapour-permeable. This property is decisive in timber frame construction: timber works with moisture, and all materials used must work with it rather than blocking the timber.

Modern building materials (densely fired bricks, sand-lime brick, cement mortar) interrupt this cycle. Moisture from the timber can no longer diffuse, collects at contact surfaces and damages the structure in the long term. Historic bricks, on the other hand, fit seamlessly into the system of timber, clay and lime: compatible in terms of building physics, coherent in material and colour, and usually preferred by monument conservation.

However, the decision between reuse and replacement does not depend on the type of material alone. The decisive factor is the condition of each individual brick. Skipping this check risks installing damaged bricks, with consequential damage that only becomes visible years later.

What is timber framing? Construction principle and material compatibility →

Check guide: these five criteria decide on reuse

Step one is a visual check for cracks and breaks. Continuous or branching cracks, broken halves and heavily chipped areas rule out reinstallation. Small chipped edges and mortar marks, on the other hand, are unproblematic. They only affect the surface, not the structural integrity of the brick.

Step two is the sound test: tap two bricks lightly against each other. A bright, clear sound shows integrity. A dull, hollow sound indicates internal cracks or frost damage. Such bricks are not reused. Step three is frost damage: flaking surfaces, bursting layers and crumbly edges are clear exclusion criteria, as frost destroys the pores irreversibly. Step four is salt contamination: white efflorescence on the surface signals dissolved salts. These bricks can still be used after complete drying but should not end up in particularly damp areas. Step five is the dimension check: large deviations in format make reuse in the bond difficult. Bricks of the same kind are kept together; formats that differ greatly are set aside for less visible areas or the interior.

As a rule of thumb: if more than one test step is negative, the brick is not reinstalled. If a single point is borderline, it may be usable with restrictions, in a less stressed position and with appropriate documentation.

Remove and clean bricks

The bricks should be removed as carefully as possible to avoid damage. If the panel was laid with clay or lime mortar, many bricks can be loosened easily. These traditional mortars remain comparatively soft and can be removed mechanically. Removal is much more difficult with cement mortar: it was used in later renovations and can be very hard, which means bricks break more often during removal.

During removal it is advisable to sort the bricks immediately: set aside well-preserved bricks, slightly damaged bricks and bricks that can no longer be used separately. This sorting makes later reinstallation considerably easier.

After removal, old mortar residues and plaster layers must be removed. The most common method is mechanical cleaning: coarse mortar residues are carefully knocked off, then smaller residues are removed with a wire brush. Dust and fine residues can then be removed with water and a brush.

A pressure washer can also be used but should be used with care. Too much pressure can damage the surface of old bricks. A moderate setting and sufficient distance from the brick are important. After cleaning, the bricks should dry completely, preferably stored on pallets with air circulating.

What role triangular battens play in timber framing

Important details when rebuilding a panel are the Triangular fillets. These small wooden battens are mounted along the timber edges and ensure a functioning transition between timber and panel infill.

Timber moves: it swells with moisture and shrinks with dryness. Brick and mortar, on the other hand, react much less to changes in moisture. If bricks are laid directly against the timber, stresses arise between the materials. These stresses lead to cracks in the panel, flaking plaster and moisture ingress at the timber. Triangular fillets ensure that the brick infill still sits firmly in the panel.

The triangular batten sits in the middle of the beam flank and, after laying, lies hidden in the mortar of the connection joint. There it holds the infill like a tongue in a groove: the timber can swell and shrink, the panel stays in place and cannot fall out. When plastering, the batten is no longer visible; the plaster is connected to the beams.

Triangular fillets usually have a leg length of about 17 to 19 millimetres and are made of larch or oak. They are nailed or screwed centrally onto the beam flanks, at least on two opposite sides.

Reinstalling the bricks and choosing the mortar

Before laying, the bricks should be moistened slightly. Dry bricks draw water from the mortar very quickly, which impairs adhesion. The bricks should be damp but not dripping wet.

Reinstallation is done step by step: apply a mortar bed, set the brick, fill joints completely, align the surface. The bricks are not set directly against the timber but end at the triangular batten.

Particularly suitable for timber frame panels are Clay mortar and lime mortar. Clay mortar was used historically and suits timber frame constructions excellently: it is capillary-active, vapour-permeable, easy to repair and very compatible with historic materials. Lime mortar, especially NHL lime, is also well suited: high vapour permeability, good strength, long durability. Cement mortar should be avoided in timber framing where possible.

After laying comes the plaster layer. Clay plaster or lime plaster is connected to the beams; at this point the triangular batten lies hidden in the masonry. The timber itself remains visible and is usually not plastered over.

Reuse or replacement: the decision rule

Reuse is recommended if most of the bricks (over 70 percent) pass the test guide, the brick format is uniform and monument conservation requirements apply. The advantages are clear: less construction waste, lower material costs, better building physics compatibility with the existing building and visual coherence with the building.

Replacement with new bricks is the right decision if more than 30 percent of the removed bricks show frost damage, cracks or irreversible salt contamination, if the brick format can no longer be obtained, or if installation is outdoors without sufficient weather protection. For external panels without a deep roof overhang, modern tested materials should be considered even if the bricks are in good condition.

Typical installation mistakes that occur regardless of the choice of material: laying bricks dry instead of pre-wetting them, Triangular fillets left out, cement mortar used, reinforcement at material transitions forgotten. These mistakes create cracks, moisture bridges and plaster damage, regardless of whether old or new bricks were installed. System knowledge of mortar choice, moisture management and connection details is more important than the origin of the material alone.

Practical examples from northern German timber frame renovations

In the Achim, Verden and Bremen area there are hundreds of timber frame houses from the 18th and 19th centuries whose panels were originally filled with fired bricks. Renovation projects show time and again that bricks hidden for decades behind cement plaster are in surprisingly good condition, provided no frost could penetrate the masonry. Anyone who keeps and checks these bricks instead of disposing of them saves material and preserves the material coherence that monument conservation wants. Especially with exposed timber framing without plaster, in this region on barns and old outbuildings, reusing historic bricks is the only way to keep a harmonious overall appearance.

Frequently asked questions about reusing bricks in timber framing

How do I decide which old bricks are reusable and which are not?

The decision depends on five specific test steps: a visual check for cracks and breaks, a sound test (clear sound = intact, dull sound = discard), a check for frost damage (flaking layers, crumbly edges), a check for salt efflorescence and a dimension check. If more than one test step is negative, the brick is not reinstalled. Individual borderline pieces can be used in a less stressed position or indoors.

When is replacement with new blocks the better decision?

If more than 30 percent of the removed bricks show frost damage, cracks or irreversible salt contamination, if the brick format can no longer be obtained, or if the bricks go into external panels without sufficient weather protection. If, on the other hand, most of the bricks, over 70 percent, pass the test guide, the format is uniform and monument conservation requirements apply, reuse is worthwhile.

What are triangular battens needed for when rebuilding a panel?

Triangular battens hold the infill in the panel. Timber moves: it swells with moisture and shrinks with dryness. Brick and mortar hardly react to changes in moisture. The battens are nailed to the middle of the beam flanks before laying and then lie hidden in the mortar of the connection joint. This keeps the panel firmly in place, even when the timber moves.

Which mortar is suitable for re-laying historic bricks in timber framing?

Clay mortar or NHL lime mortar. Clay mortar is capillary-active, vapour-permeable, easy to repair and suits historic timber frame constructions. NHL lime offers good strength with high vapour permeability. You should avoid cement mortar in timber framing because it traps moisture and damages the timber in the long term. Moisten the bricks lightly before laying so that they do not draw water from the mortar too quickly.

Created by Kenny Kent Bridgewater, certified expert for resource-efficient and sustainable building with clay building materials. Clay building, timber construction and life cycle assessment in northern Germany. Advice from the author →

To take away: the free clay building diary with drying log.